The mechanical properties are almost identical to traditionally manufactured copper.
TABLE
Tensile strength |
210 – 230 MPa |
Yield strength |
120 – 160 MPa |
Elongation at break |
40 – 60 % |
Young’s modulus |
110 GPa |
The mechanical properties are almost identical to traditionally manufactured copper.
TABLE
Tensile strength |
210 – 230 MPa |
Yield strength |
120 – 160 MPa |
Elongation at break |
40 – 60 % |
Young’s modulus |
110 GPa |